Polymer Property : Viscosity = 190000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 190000 - 190000 cP

@Temperature 280 - 280 °C
190000 - 190000 cP

@Temperature 536 - 536 °F
Average value: 190000 cP Grade Count:2
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..
Viscosity 190000 - 190000 cP

@Shear Rate 1000 - 1000 1/s
190000 - 190000 cP

@Shear Rate 1000 - 1000 1/s
Average value: 190000 cP Grade Count:2
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..