Polymer Property : Viscosity = 18800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 18800 cP

@Temperature 25.0 °C
18800 cP

@Temperature 77.0 °F
Cytec EN-2527 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..