Viscosity 1686 cP

@Temperature 23.0 °C
1686 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® EK2000 Epoxy
Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance ..