Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 162 cP | 162 cP | |
LG Chemical TOTM Plasticizer Features: LG TOTM is used in cable and sheet by product that aging property and migration resistance among our products are superior.Application: Power cableInformation provided by LG Chemical |