Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1493 cP | 1493 cP | Part A |
3M Scotch-Weld™ DP604NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the .. |