Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 145200 cP @Shear Rate 5000 1/s, Temperature 220 °C |
145200 cP @Shear Rate 5000 1/s, Temperature 428 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010