Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 14 cP | 14 cP | D=30/s; DIN 54 453 |
3M Dyneon™ TF 5035 PTFE Dispersion
(discontinued **) Used for metal coatings; impregnation.Dyneon PTFE dispersions are aqueous dispersions developed for use in metal coating formulations and for application of impregnation and fabric coating applicat.. |
|||
Viscosity | 14 cP | 14 cP | dynamic |
Dow Corning 3037 INTERMEDIATE Reactive silicone intermediate for coil coatings, appliance finishes and other finishes where improved heat or weathering resistance is needed. Typically reacted with saturated polyesters or oil-fre.. |