Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 13700 cP @Shear Rate 11200 1/s, Temperature 200 °C |
13700 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |