Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 13 - 18 cP | 13 - 18 cP | |
Huntsman Araldite RD-2 Reactive Diluent Weight per Epoxide (EEW, g/eq) 120 to 135. Max color is 1.Comments/Applications: 1,4 butanediol diglycidyl ether - difunctional epoxy. Versus RD-1 - gives higher flashpoint (280°F vs. 120°F).. |
|||
Viscosity | 13 - 16 cP @Temperature 20.0 °C |
13 - 16 cP @Temperature 68.0 °F |
4% solids aqueous solution, Hoeppler falling ball method |
DuPont Elvanol® 70-14 Polyvinyl Alcohol Intermediately Hydrolyzed General Purpose Grade Elvanol® polyvinyl alcohol (PVOH) is used in the manufacture of spiral wound tubes, coated paper and linerboard, and specialty water-soluble films. Its higher binding capacity versus synthetic late.. |