Polymer Property : Viscosity = 1280 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 780 - 1280 cP

@Temperature 125 °C
780 - 1280 cP

@Temperature 257 °F
542-111
Westlake Epolene® N-30 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer
Product Description: Epolene N-30 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss..