Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 117 cP @Temperature 25.0 °C |
117 cP @Temperature 77.0 °F |
Solution Viscosity in 5 wt.% Toluene; UBE Method |
UBE UBEPOL BR230 Non-Oil Extended Synthetic Rubber (Raw Polymer) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Microstructure: cis: 97.8trans: 1.1vinyl: 1.1Information provided by UBE. |