Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 115 - 135 cP | 115 - 135 cP | |
Ritelok TL41 Oil Tolerant Threadlocker Anaerobic. Medium strength threadlocker. Designed to lock oily fasteners. Prevent corrosion, Vibration resistant, Dismantle using normal tools |