Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 114000 cP | 114000 cP | Base |
ACC QM 260 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 260 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |