Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 104000 cP @Shear Rate 300 1/s, Temperature 190 °C |
104000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys DuraGrip™ DGR 6070 NC Thermoplastic Elastomer (TPE) DuraGrip® DGR 6070NC is designed to be a general purpose Thermoplastic Elastomer (TPE) that is easy to use in injection molding and extrusion processes. DGR 6070NC has an
excellent soft touch feel,.. |
|||
Viscosity | 104000 cP @Shear Rate 300 1/s, Temperature 190 °C |
104000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys DuraGrip™ 6870 Thermoplastic Elastomer With its true rubber look and feel, DuraGrip® TPE improves the performance and appearance of virtually any consumer or light industrial product. Its one of the most versatile materials in APAs exte.. |