Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 101 - 300 cP | 101 - 300 cP | ASTM D445 |
IRPC Polimaxx Polene PE250N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |