Physical Properties Metric English Comments
Viscosity 300000 - 1.90e+6 cP

@Temperature 190 - 190 °C
300000 - 1.90e+6 cP

@Temperature 374 - 374 °F
Average value: 495000 cP Grade Count:22
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..
Viscosity 300000 - 1.90e+6 cP

@Shear Rate 50.0 - 50.0 1/s
300000 - 1.90e+6 cP

@Shear Rate 50.0 - 50.0 1/s
Average value: 495000 cP Grade Count:22
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade". Each property range of values reported ..