Polymer Property : Viscosity = 1.80e+6 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1.80e+6 - 2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 232 °C
1.80e+6 - 2.10e+6 cP

@Shear Rate 100 1/s,
Temperature 450 °F
Melt; ASTM D3835
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong..
Viscosity 1.80e+6 cP
1.80e+6 cP
A
Shin-Etsu Silicones LIMSâ„¢ KEG2000-40A/B Elastomer
KEG2000-40 is a fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to..