Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.45 - 1.75 cP | 1.45 - 1.75 cP | |
Dow Corning XIAMETER® PMCPPMX-1184 Silicone Fluid Is chemically equivalent to DOW CORNING® 2-1184 FLUID. A mixture of volatile linear polydimethylsiloxane for use in skincare, suncare, color cosmetic, haircare, and antiperspirant / deodorant appli.. |