Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.7 cP @Temperature 25.0 °C |
1.7 cP @Temperature 77.0 °F |
|
LyondellBasell NMP N-methyl-2-pyrrolidone Available in electronic grade.Information provided by Lyondell. |
|||
Viscosity | 1.7 cP | 1.7 cP | Ubbelohde viscosity meter |
BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS) ONGROSTYR F-I is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e... |
|||
Viscosity | 1.7 cP | 1.7 cP | Ubbelohde viscosity meter |
BorsodChem ONGROSTYR F-IV Expandable Polystyrene (EPS) ONGROSTYR F-IV is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |
|||
Viscosity | 1.7 cP | 1.7 cP | |
BASF 2- Ethylhexyl Acrylate Formula: C11H20O2CAS: 203-080-7Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: 2-Ethylhexyl acrylate forms homopolymers and copolymers. .. |
|||
Viscosity | 1.7 cP | 1.7 cP | Ubbelohde viscosity meter |
BorsodChem ONGROSTYR F-II Expandable Polystyrene (EPS) ONGROSTYR F-II is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e.. |
|||
Viscosity | 1.7 cP | 1.7 cP | Ubbelohde viscosity meter |
BorsodChem ONGROSTYR F-III Expandable Polystyrene (EPS) ONGROSTYR F-III is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i... |