Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.57e+6 cP @Temperature 130 °C |
1.57e+6 cP @Temperature 266 °F |
Melt; ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 500 Linear Thermoplastic Polyurethane Pearlbond™ 500 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a high crystallization rate and a very high thermoplasticity level.Appli.. |