Physical Properties Metric English Comments
Viscosity 1.55e+6 cP
1.55e+6 cP
Melt Viscosity, 240°C, 100 sec-1; ASTM D3825
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant.
Viscosity 1.55e+6 cP
1.55e+6 cP
Melt Viscosity, 240°C, 100 sec-1; ASTM D3825
SABIC Innovative Plastics Cycolac® EX58 ABS (Europe-Africa-Middle East)
High impact ABS for sheet extrusion and blow molding applications.