Viscosity 1.45e+6 cP

@Temperature 260 °C
1.45e+6 cP

@Temperature 500 °F
Melt Viscosity; DSM Method
DSM Akulon® XP32-E1 PA6
Film Extrusion, Medium Viscosity, Lubricated, Nucleated