Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.3 cP | 1.3 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® NVW PVC PVC Homopolymer Dispersion Resin F-NVW is a high molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Plastisols containing F-NVW exhibit low paste viscosities and.. |
|||
Viscosity | 1.3 cP | 1.3 cP | dynamic |
Dow Corning OS-30 Information provided by Dow Corning |
|||
Viscosity | 1.3 cP | 1.3 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® NVA PVC PVC Homopolymer Dispersion Resin F-NVA is a high molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Plastisols containing F-NVA exhibit low paste viscosities and.. |