Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.12 cP | 1.12 cP | Inherent; ASTM D1243 |
Formosa Plastics Formolon® 25 PVC PVC Homopolymer Dispersion Resin F- 25 is a medium molecular weight PVC homopolymer dispersion resin with low residual surfactant content. Applications include caulk and sealants.Note 1. 500 gm resi.. |