Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.02 - 2.51 cP | 1.02 - 2.51 cP | Average value: 1.73 cP Grade Count:6 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Viscosity | 1.02 cP | 1.02 cP | Inherent; ASTM D5225 |
Formosa Plastics Formolon® 680 PVC Homopolymer General Purpose Grade Resin F680 is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, thi.. |
|||
Viscosity | 1.02 cP | 1.02 cP | Inherent; ASTM D5225 |
Formosa Plastics Formolon® 680H PVC Homopolymer General Purpose Grade Resin F680H is especially suited for processing from powder blends due to its ability to rapidly absorb plasticizers regardless of molecular weight. In addition, th.. |
|||
Viscosity | 1.02 cP | 1.02 cP | Inherent; ASTM D5225 |
Formosa Plastics Formolon® 680M PVC Homopolymer General Purpose Grade Resin F680M is a medium molecular weight PVC homopolymer suitable for both rigid and flexible applications and is low in gels and finds acceptance in calendered fil.. |
|||
Viscosity | 1.02 cP | 1.02 cP | Inherent; ASTM D5225 |
Formosa Plastics Formolon® 685 PVC Homopolymer General Purpose Grade Resin F685 is especially suited for processing from powder blends due to its ability to absorb plasticizers regardless of molecular weight. In addition, this produc.. |