Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 1.00e+15 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Average value: 5.05e+14 cP Grade Count:12
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Molded". Each property range of values reported is minimum and maximum v..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Average value: 5.05e+14 cP Grade Count:10
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON F-104 PTFE Fine Powder
Processing Methods: Paste extrusion, calendering.Applications: Unsintered tape, sealing tape, low specific gravity tape, tape for wrapping flat cables, tubes.Information provided by Daikin Industrie..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON F-201 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON F-205 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Spaghetti tubes, small diameter tubes, fine electric wire smaller than AGW16.Information provided by Daikin Industries.
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON F-302 PTFE Fine Powder
Processing Methods: Paste extrusion.Applications: Small to large diameter tubes, flexible hoses, shrinkable tubes, heavy duty electric wires smaller than AGW18, and jackets.Information provided by ..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-112 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with especially good elasticity, making it ideal for molding diaphragms and bellows. Offers excellent post-moldin..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-12 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Useful in making products requiring fine texture, especially insulation skiving tapes. Also allows uniform mixing of inorganic fill..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-139 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic compression molding.Features: Excellent fluidity. Apparent density is large and ideal for automated compression molding proces..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut
Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic or semi-automatic compression molding, isostatic molding, and ram extrusion.Features: Good fill characteristics particularly into ..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON M-393 PTFE Molding Powder, Free Flow
Free flow powder.Processing Methods: Compression molding, automatic compression molding, and ram extrusion.Features: Maximum emphasis given to ease of handling during molding. Used when molded arti..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1030 PTFE 15% Glass Fiber Filled Molding Powder
15% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1040 PTFE 20% Glass Fiber Filled Molding Powder
20% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1040F PTFE 20% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder
20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1241F PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder, High Apparent Density, Free Flow
20% glass fiber and 5% graphite filled. High apparent density and free-flowing properties. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1431 PTFE 15% Glass Fiber and 5% MoS2 Filled Molding Powder
15% glass fiber and 5% MoS2 filled. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanical and electrical service (e.g. split-curled bearings..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1431F PTFE 20% Glass Fiber and 5% MoS2 Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber and 5% MoS2 filled. High apparent density and free-flowing properties. High wear resistance, good electrical properties, low friction, high creep resistance.Applications: Mechanica..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder
15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder
30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-6030 PTFE 15% Carbon Fiber Filled Molding Powder
15% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-6050 PTFE 25% Carbon Fiber Filled Molding Powder
25% carbon fiber filled. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechanical seals and bearing pads)Information provided by ..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1030F PTFE 15% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow
15% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl..
Viscosity 1.00e+13 - 1.00e+15 cP

@Temperature 340 - 380 °C
1.00e+13 - 1.00e+15 cP

@Temperature 644 - 716 °F
Melt viscosity
Daikin POLYFLON MG-1050 PTFE 25% Glass Fiber Filled Molding Powder
25% glass fiber filled. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Available in all forms (e.g. bearings, gaskets, valve seats,..
Copyright © lookpolymers.com All Rights Reserved