Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.92 cP | 0.92 cP | Inherent; ASTM D5225 |
Formosa Plastics Formolon® 622 PVC Homopolymer Pipe Grade Resin F622 is a medium-low molecular weight PVC homopolymer designed primarily for rigid extrusion applications. This product has excellent dry flow characteristics, making i.. |