Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.81 cP | 0.81 cP | Inherent; ASTM D5225 |
Formosa Plastics Formolon® 622R PVC Homopolymer General Purpose Grade Resin F622R is a medium-low molecular weight PVC homopolymer of interest in both rigid and flexible applications and has established a deserved reputation for low .. |
|||
Viscosity | 0.81 - 0.85 cP | 0.81 - 0.85 cP | Intrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista |
Invista 1101R Copolymer Packaging Resin
(discontinued **) Carboxyl end groups: |