Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.58 cP | 0.58 cP | |
3M Novec™ 7100DL Engineered Fluid A higher purity version of 3M™ Novec™ 7100, 3M™ Novec™ 7100DL is tightly-controlled for ions, metals and non-volatile residue. It is used in precision cleaning and deposition applications when h.. |
|||
Viscosity | 0.58 cP | 0.58 cP | |
3M Novec™ 7200DL Engineered Fluid A high-purity version of 3M™ Novec™ 7200, 3M™ Novec™ 7200DL is tightly-controlled for ions, metals and non-volatile residue. It is used when an application calls for high-purity materials, or a .. |