Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 8.7 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.7 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow DX5E66 Polypropylene Homopolymer Resin OverviewConsistent processabilityVery high cleanlinessGood optical propertiesComplies with U.S. FDA 21 CFR 177.1520 (c)1.1a, EU-Directive 2002/72/EC, Canadian HPFB No ObjectionDX5E66 Developmental P.. |