Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Melt Index of Compound | 8.5 g/10 min | 8.5 g/10 min | MFI 5kg/200°C; Finaprene 1006 Method |
Total Finaprene® 602 Thermoplastic Elastomer
(discontinued **) Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer (SBS). Thanks to is broad molecular weight distribution, Finaprene® 602 provides good fluidity properties.. |
|||
Melt Index of Compound | 8.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238G |
Total Finaprene® 602D Clear Impact Polystyrene
(discontinued **) Finaprene® 602D is a clear high styrenic styrene-butadiene (SBS) block copolymer with a radial structure, which is widely used as modifiers or in alloys with many plastic resins, such polystyrene, .. |
|||
Melt Index of Compound | 8.5 g/10 min @Load 21.6 kg, Temperature 150 °C |
8.5 g/10 min @Load 47.6 lb, Temperature 302 °F |
Fainplast |
Fainplast Compounds HAX HF 045 Halogen Free PVC General purpose; improved fire performance |