Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 7.35 g/10 min @Load 10.0 kg, Temperature 220 °C |
7.35 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
LG Chemical PI-642 ABS, Fitting, High Strength Information Provided by LG Chem |