Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 6.7 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.7 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 115-1333 LMDPE Rotational Molding Resin Description: ICORENE 115-1333 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |