Polymer Property : Melt Index of Compound = 59 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 59 g/10 min

@Load 5.00 kg,
Temperature 190 °C
59 g/10 min

@Load 11.0 lb,
Temperature 374 °F
MVR, [cm<sup>3</sup>/10 min]
Huntsman IROGRAN® CA116-203 TPU-Polyester
Introduction: IROGRAN CA116-203 is a high performance polyester based thermoplastic polyurethane intended for flat die extrusion applications. IROGRAN CA116-203 is part of the HUNTSMAN film and shee..
Melt Index of Compound 59 g/10 min

@Load 10.0 kg,
Temperature 220 °C
59 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall
Information Provided by LG Chem