Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 5.75 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.75 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |