Polymer Property : Melt Index of Compound = 5.7 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 5.7 g/10 min

@Temperature 230 °C
5.7 g/10 min

@Temperature 446 °F
ASTM D1238
Mitsui ADMER® QF551A PP Type Polyolefin
ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar..