Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 5.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 115-1008 LMDPE Rotational Molding Resin Description: ICORENE 115-1008 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Melt Index of Compound | 5.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 115-1650 LMDPE Rotational Molding Resin Description: ICORENE 115-1650 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Melt Index of Compound | 5.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 115-1653 LMDPE Rotational Molding Resin Description: ICORENE 115-1653 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |