Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 49 g/10 min @Load 10.0 kg, Temperature 300 °C |
49 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |