Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Index of Compound = 28 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Index of Compound 28 g/10 min

@Load 10.0 kg,
Temperature 220 °C
28 g/10 min

@Load 22.0 lb,
Temperature 428 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific)
Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated.
Melt Index of Compound 28 g/10 min

@Load 21.6 kg,
Temperature 190 °C
28 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
Melt Index of Compound 28 g/10 min

@Load 5.00 kg,
Temperature 360 °C
28 g/10 min

@Load 11.0 lb,
Temperature 680 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.
Melt Index of Compound 28 g/10 min

@Load 2.16 kg,
Temperature 190 °C
28 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Sterigenics Raprex® R-400C Thermoplastic Powder
Applications: Extrusion CoatingsA thermoplastic powder based on polyethylene was developed by Sterigenics Advanced Applications for extrusion coating on metal and other surfaces. RAPREXâ„¢ 400 is..
Melt Index of Compound 28 g/10 min

@Load 5.00 kg,
Temperature 300 °C
28 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific)
LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform..
Melt Index of Compound 28 g/10 min

@Load 5.00 kg,
Temperature 224 °C
28 g/10 min

@Load 11.0 lb,
Temperature 435 °F
ASTM D1238
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer  (discontinued **)
Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in..