Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 210 - 260 g/10 min | 210 - 260 g/10 min | |
Zig Sheng Industrial ZISAMIDE® HP3207 Nylon 6 ZISAMIDE® HP3207 is a spinning grade Polyamide 6. Application: textile brightInformation provided by ZIG SHEN Industrial Co., LTD. |