Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 2.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical HI835S PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Melt Index of Compound | 2.6 g/10 min @Temperature 190 °C |
2.6 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® SF755A Elastomer Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |