Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 130 - 180 g/10 min | 130 - 180 g/10 min | |
Zig Sheng Industrial ZISAMIDE® TP4209 Nylon 6 ZISAMIDE® TP4209 is a Polyamide 6. Application: compounding injectionInformation provided by ZIG SHEN Industrial Co., LTD. |