Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 10 - 17 g/10 min | 10 - 17 g/10 min | |
Sibur ABS 1530 Molding Grade ABS Plastic Thermal resistance with higher fluidity for large and thin wall articles. |
|||
Melt Index of Compound | 14 - 17 g/10 min | 14 - 17 g/10 min | II Preparation |