Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 90 - 140 g/10 min | 90 - 140 g/10 min | |
Zig Sheng Industrial ZISAMIDE® HP3401 Nylon 6 ZISAMIDE® HP3401 is a spinning grade Polyamide 6. Application: textile brightInformation provided by ZIG SHEN Industrial Co., LTD. |