Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.65 g/10 min | 1.65 g/10 min | |
Lushan WR-2 Wood Plastic Composites Compatibilizer Compatibilizer/coupling agent Lushan series for wood plastic composites is a maleic anhydride grafted polyolefins, applied in PE, PVC, wood powder, and bamboo powder and wood fiber composite materia.. |