Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.66 g/10 min | 0.66 g/10 min | ASTM D1238 |
Amco PRIMATOP HDPE 006964EG Pipe Extrusion Polyethylene HDPE 006964 features high quality for critical food packaging requirements and excellent stiffness. Applications include milk, water, and juice packaging.Former A-Top Polymers product; part of Amco .. |