Physical Properties Metric English Comments
Melt Index of Compound 0.65 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is als..
Melt Index of Compound 0.65 g/10 min
0.65 g/10 min
ASTM D1238
Amco PRIMATOP HDPE 006964 Blow Molding Polyethylene
HDPE 004955HP features excellent stiffness to ESCR ratio and good impact resistance. Applications include oil bottles, household and industrial chemical containers, and personal care products.Former..