Physical Properties Metric English Comments
Melt Index of Compound 0.38 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.38 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol..
Melt Index of Compound 0.38 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.38 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol..