Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0413 cm/cm @Thickness 3.17 mm |
0.0413 in/in @Thickness 0.125 in |
Direction of Flow; ASTM D955 |
Diamond Polymers Softflex® 1302 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |