Linear Mold Shrinkage 0.038 cm/cm

@Thickness 3.17 mm
0.038 in/in

@Thickness 0.125 in
Transverse to Flow; ASTM D955
Diamond Polymers Softflex® 1302 Thermoplastic Elastomer Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.